    I'm new to lost wax casting using 3D printed resins. I'm starting with Powerresins "Dark" 3D castable resin. The burnout cycle is at the link.

    Question: Is it possible/recommended to use multiple day burnouts with castable resins in general, especially the Powerresins "Dark" resin? I.e. Run the 5 hours at 150c on one day, let the mold cool inside the kiln, and then do the high temperature burnout the next day (assuming a long temperature run up?)

  2. #2
    Join Date
    Mar 2011
    Location
    Manchester UK
    Posts
    951

    Default

    I think you would need to ask the investment people that question as its the investment that will suffer. I do it all in one go but I don't really see a problem theoretically ?